Fe2(MoO4)3超细微粒催化剂的制备

匡文兴,范以宁,陈开东,王净雷,陈懿   

  1. 南京大学化学系,南京 210093
  • 收稿日期:1996-06-28 修回日期:1996-10-11 发布日期:1997-01-15
  • 通讯作者: 匡文兴

Preparation of Fe2(MoO4)3 Ultrafine Particle Catalyst

Kuang Wen-Xing,Fan Yi-Ning,Chen Kai-Dong,Wang Jing-Lei,Chen Yi   

  1. Department of Chemistry,Nanjing University,Nanjing 210093
  • Received:1996-06-28 Revised:1996-10-11 Published:1997-01-15
  • Contact: Kuang Wen-Xing

关键词: Fe2(MoO4)3, 超细微粒, 溶胶-凝胶法

Abstract:

Fe2(MoO4)3 ultrafine particle catalyst has been prepared successfully by the sol-gel process at lower temperature. The influences of preparation conditions and thermal treatment conditions on the morphology and structure of the ultrafine particle catalyst has been studied by using TEM, DTA-TG, FT-IR, XRD and BET surface area measurement methods. It is shown that the BET surface area of Fe2(MoO4)3 ultrafine particle prepared by sol-gel method is much larger than that of Fe2(MoO4)3 prepared by coprecipitation method. For the preparation of the well-distribuated Fe2(MoO4)3 ultrafine particles with the size in the range of 40-80nm, the optimum conditions are : treatment temperature <=673K, L/M (Citric acid/Metallic ions)=0.3 and pH<1.0.