Acta Phys. -Chim. Sin.  2012, Vol. 28 Issue (01): 137-145    DOI: 10.3866/PKU.WHXB201228137
ELECTROCHEMISTRY AND NEW ENERGY     
Adsorption Mechanism of Nicotinic Acid onto a Passive Iron Surface
TIAN Hui-Wen1,2, LI Wei-Hua1, WANG Da-Peng3, HOU Bao-Rong1
1. Key Laboratory of Corrosion Science in Shandong, Institute of Oceanology, Chinese Academy of Sciences, Qingdao 266071, Shandong Province, P. R. China;
2. Graduate University of Chinese Academy of Sciences, Beijing 100049, P. R. China;
3. Key Laboratory of Rubber-Plastics of Ministry of Education and Shandong Province, Qingdao University of Science & Technology, Qingdao 266042, Shandong Province, P. R. China
Download:   PDF(1151KB) Export: BibTeX | EndNote (RIS)      

Abstract  Cyclic voltammetry and in situ Raman spectroscopy were used to determine the adsorption mechanism of nicotinic acid onto passive iron film surface. Its ability to form a surface complex tends to stabilize the interstitial Fe in Fe states and results in the progressive development of an insoluble film. Furthermore, an analytical investigation using a rotating electrochemical quartz crystal microbalance (rEQCM) showed that the adsorption isotherms of nicotinic acid onto iron in the active and passive states followed Langmuir-Freundlich behavior from which the adsorption constant, standard free energy of adsorption, and heterogeneity could be calculated. The organic molecules attach to the film surface by chemisorption and the interstitial cations are fixed in the octahedral sites giving stable nanocrystals. These assumptions were confirmed by scanning electron microscopy (SEM) and attenuated total reflection transform infrared (ATR FTIR) spectroscopy.

Key wordsNicotinic acid      Passive film on iron      Alkaline medium      Adsorption     
Received: 30 June 2011      Published: 17 October 2011
MSC2000:  O646  
Fund:  

The project was supported by the National Natural Science Foundation of China (51179182), Shinan Scientific and Technological R&D Foundation of Qingdao City, China (P2010-1-ZH-005), Ph.D. Foundation of Shandong Province, China (BS2009HZ002), and K. C.Wong Education Foundation, Hong Kong, China (20061231).

Corresponding Authors: LI Wei-Hua     E-mail: liweihua@qdio.ac.cn
Cite this article:

TIAN Hui-Wen, LI Wei-Hua, WANG Da-Peng, HOU Bao-Rong. Adsorption Mechanism of Nicotinic Acid onto a Passive Iron Surface. Acta Phys. -Chim. Sin., 2012, 28(01): 137-145.

URL:

http://www.whxb.pku.edu.cn/10.3866/PKU.WHXB201228137     OR     http://www.whxb.pku.edu.cn/Y2012/V28/I01/137

(1) Söylev, T. A.; Richardson, M. G. Constr. Build. Mater. 2008, 22, 609.  
(2) Jussain, R.; Ishida, T. Constr. Build. Mater. 2011, 25, 1305.  
(3) Chen,W.; Du, R.; Ye, C. Electrochim. Acta 2010, 55, 5677.  
(4) Wei, J.; Dong, J.; Ke,W. Constr. Build. Mater. 2011, 25, 1243.  
(5) Ann, K. J.; Jung, H. S.; Kim, H. S. Cem. Concr. Res. 2006, 36, 530.  
(6) Garcés, P.; Saura, P.; Méndez, A. Corrosion Sci. 2008, 50, 498.  
(7) Sanchez, M.; Alonso, M. Constr. Build. Mater. 2011, 25, 873.  
(8) Al-Mehthel, M.; Dulaijan, S. Construc. Build. Mater. 2009, 23, 1768.  
(9) Ormellese, M.; Lazzari, L.; Goidanich, S.; Fumagalli, G.; Brenna, A. Corrosion Sci. 2009, 51, 2959.  
(10) Jamil, H. E.; Shriri, A.; Boulif, R. Cem. Concr. Comp. 2005, 27, 671.  
(11) Jamil, H. E.; Shriri, A.; Boulif, R. Electrochim. Acta 2004, 49, 2753.  
(12) Ferreira, E. S.; Giacomelli, C.; Spinelli, A. Mat. Chem. Phys. 2004, 83, 129.  
(13) Goncalves, R. S.; Mello, L. D. Corrosion Sci. 2001, 43, 457.  
(14) Akrout, H.; Bousselmi, L.; Dalard, F. J. Mater. Sci. 2004, 39, 7341.  
(15) Valek, L.; Martinez, S.; Brnardi?, I. Corrosion Sci. 2008, 50, 2705.  
(16) Martinez, S.; Valek, L.; Oslakovi?, I. S. J. Electrochem. Soc. 2007, 11, C671.
(17) Valek, L.; Martinez, S.; Serdar, M.; Oslakovi?, I. S. Chem. Biochem. Eng. Q. 2007, 21, 65.
(18) Soylev, T.; McNally, C. Cem. Concr. Res. 2007, 37, 972.  
(19) Soylev, T.; McNally, C. Cem. Concr. Res. 2007, 29, 357.  
(20) Trabanelli, G.; Monticelli, C.; Grassi, V. Cem. Concr. Res. 2005, 35, 1804.  
(21) Mechmeche, L. B.; Dhouibi, L.; Zucchi, F. Cem. Concr. Compos. 2008, 30,167.  
(22) Qu, Q.; Li, L.; Ding, Z. Corrosion Sci. 2009, 51, 2423.  
(23) Elsener, B. Corrosion Inhibitors for Steel in Concrete. In: International Congress of Advanced Materials, Their Processes and Applications, Munich, Germany, Aug 5-10, 2000.
(24) Ormellese, M.; Taffaini, G.; Ganazzoli, F. Corrosion 2009, 3, 22.
(25) Diamanti, M. V.; Ormellese, M.; Pedeferri, M. Cem. Concr. Res. 2008, 38, 1349.  
(26) Ju, H.; Li, Y. Corrosion Sci. 2007, 49, 4185.  
(27) Ju, H.; Kai, Z.; Li, Y. Corrosion Sci. 2008, 50, 865.  
(28) Taylor, H. Cement Chemistry, 2nd ed.; T. Telford Pub.: London, 1998; p 214.
(29) Marinkovi?, N. S.; Calvente, J. J.; Ková?ová, Z. J. Electrochem. Soc. 1996, 143, L171.
(30) Ahlberg, E.; Friel, M. J. Electrochem. Soc. 1990, 137, 1196.  
(31) Kern, P.; Landolt, D. J. Electrochem. Soc. 2000, 147, 318.  
(32) Kern, P.; Agarwal, P.; Landolt, D. Design and Characterization of A Rotating Electrochemical Quartz-crystal-microbalance Electrode. German Patent DE 19911291 C2, 2001-09-21.
(33) Vatankhah, G.; Lessard, J.; Jerkiewicz, G. Electrochim. Acta 2003, 48, 1619.
(34) Méndez, A.; Diaz-Arista, P.; Trejo, G. Int. J. Electrochem. Sci. 2008, 3, 918.
(35) Kern, P.; Landolt, D. Electrochim. Acta 2001, 47, 589.  
(36) Kern, P.; Landolt, D. J. Electrochem. Soc. 2001, 148, B228.
(37) McCafferty, E. J. Electrochem. Soc. 1999, 146, 2863.  
(38) Kern, P.; Landolt, D. J. Electroanal. Chem. 2001, 500, 170.  
(39) Joiret, S.; Keddam, M.; Takenouti, H. Cem. Concr. Compos. 2002, 24, 7.  
(40) Dubois, F.; Mendibide, C.; Pagnier, T. Corrosion Sci. 2008, 50, 3401.  
(41) Xiao, K.; Dong, C.; Li, X. J. Iron steel Res. Int. 2008, 15, 42.
(42) McHale, J. M.; Auroux, A.; Perrotta, A. J. Science 1997, 277, 788.  
(43) Davenport, A. J.; Oblonsky, L. J.; Ryan, M. P. J. Electrochem. Soc. 2000, 147, 2162.  
(44) MacDonald, D. D.; Sun, A. Electrochim. Acta 2006, 51, 1767.  
(45) Zhang, Y.; MacDonald, D. D.; MacDonald, M. U. Corrosion Sci. 2006, 48, 3812.  
(46) Diáz, B.; Joiret, S.; Nóvoa, X. R. Electrochim. Acta 2004, 49, 3039.  
(47) Hamadou, L.; Kadri, A.; Benbrahim, N. Appl. Surf. Sci. 2005, 252, 1510.  
(48) Tajmir-Riahi, H. A. J. Inorg. Biochem. 1991, 42, 47.  
(49) Tajmir-Riahi, H. A. J. Inorg. Biochem. 1991, 44, 39.  
(50) Paul, R. C.; Mohini, C.; Chadha, S. L. Transition Met. Chem. 1981, 6, 300.  
(51) Chang, H. C.; Matijevi?, E. J. Colloid Interface Sci. 1983, 92, 479.  
(52) Das, C. M.; Sudersanan, M. J. Appl. Electrochem. 2003, 33, 333.  
(53) Martell, A. E.; Smith, R. M. Critical Stability Constants; Plenum: London, 1974.
(54) Martinez, S.; Stern, I. Chem. Biochem. Eng. Q. 1999, 13, 191.
(55) Sauerbrey, G. Z. Phys. 1959, 155, 206.  
(56) Gan, F.; Dai, Z.;Wang, D. Corrosion Sci. 2000, 42, 1379.  
(57) Olsson, C.; Agarwal, P.; Landolt, D. Corrosion Sci. 2000, 42, 1197.  
(58) Kern, P.; Landolt, D. Corrosion Sci. 2002, 44, 1809.  
(59) Toney, M. F.; Davenport, A. J.; Oblonsky, L. J. Phys. Rev. Lett. 1997, 79, 4282.  
(60) Li,W.; He, Q.; Hou, B. Electrochim. Acta 2007, 22, 6386.
[1] GU Yuxing, YANG Juan, WANG Dihua. Electrochemical Features of Carbon Prepared by Molten Salt Electro-reduction of CO2[J]. Acta Phys. -Chim. Sin., 2019, 35(2): 208-214.
[2] Jyotirmoy DEB,Debolina PAUL,David PEGU,Utpal SARKAR. Adsorption of Hydrazoic Acid on Pristine Graphyne Sheet: A Computational Study[J]. Acta Phys. -Chim. Sin., 2018, 34(5): 537-542.
[3] Xuanjun WU,Lei LI,Liang PENG,Yetong WANG,Weiquan CAI. Effect of Coordinatively Unsaturated Metal Sites in Porous Aromatic Frameworks on Hydrogen Storage Capacity[J]. Acta Phys. -Chim. Sin., 2018, 34(3): 286-295.
[4] Yuan DUAN,Mingshu CHEN,Huilin WAN. Adsorption and Activation of O2 and CO on the Ni(111) Surface[J]. Acta Phys. -Chim. Sin., 2018, 34(12): 1358-1365.
[5] Qiang LIU,Yong HAN,Yunjun CAO,Xiaobao LI,Wugen HUANG,Yi YU,Fan YANG,Xinhe BAO,Yimin LI,Zhi LIU. In-situ APXPS and STM Study of the Activation of H2 on ZnO(10${\rm{\bar 1}}$0) Surface[J]. Acta Phys. -Chim. Sin., 2018, 34(12): 1366-1372.
[6] Chen-Hui ZHANG,Xin ZHAO,Jin-Mei LEI,Yue MA,Feng-Pei DU. Wettability of Triton X-100 on Wheat (Triticum aestivum) Leaf Surfaces with Respect to Developmental Changes[J]. Acta Phys. -Chim. Sin., 2017, 33(9): 1846-1854.
[7] Chan YAO,Guo-Yan LI,Yan-Hong XU. Carboxyl-Enriched Conjugated Microporous Polymers: Impact of Building Blocks on Porosity and Gas Adsorption[J]. Acta Phys. -Chim. Sin., 2017, 33(9): 1898-1904.
[8] Zhou-Sheng MO,Yu-Cai QIN,Xiao-Tong ZHANG,Lin-Hai DUAN,Li-Juan SONG. Influencing Mechanism of Cyclohexene on Thiophene Adsorption over CuY Zeolites[J]. Acta Phys. -Chim. Sin., 2017, 33(6): 1236-1241.
[9] Wei-Guo DAI,Dan-Nong HE. Selective Photoelectrochemical Oxidation of Chiral Ibuprofen Enantiomers[J]. Acta Phys. -Chim. Sin., 2017, 33(5): 960-967.
[10] Lei HE,Xiang-Qian ZHANG,An-Hui LU. Two-Dimensional Carbon-Based Porous Materials: Synthesis and Applications[J]. Acta Phys. -Chim. Sin., 2017, 33(4): 709-728.
[11] Fang CHENG,Han-Qi WANG,Kuang XU,Wei HE. Preparation and Characterization of Dithiocarbamate Based Carbohydrate Chips[J]. Acta Phys. -Chim. Sin., 2017, 33(2): 426-434.
[12] Tao-Na ZHANG,Xue-Wen XU,Liang DONG,Zhao-Yi TAN,Chun-Li LIU. Molecular Dynamics Simulations of Uranyl Species Adsorption and Diffusion Behavior on Pyrophyllite at Different Temperatures[J]. Acta Phys. -Chim. Sin., 2017, 33(10): 2013-2021.
[13] Jun-Jun CHEN,Cheng-Wu SHI,Zheng-Guo ZHANG,Guan-Nan XIAO,Zhang-Peng SHAO,Nan-Nan LI. 4.81%-Efficiency Solid-State Quantum-Dot Sensitized Solar Cells Based on Compact PbS Quantum-Dot Thin Films and TiO2 Nanorod Arrays[J]. Acta Phys. -Chim. Sin., 2017, 33(10): 2029-2034.
[14] Shao-Zheng ZHANG,Jia LIU,Yan XIE,Yin-Ji LU,Lin LI,Liang LÜ,Jian-Hui YANG,Shi-Hao WEI. First-Principle Study of Hydrogen Evolution Activity for Two-dimensional M2XO2-2x(OH)2x (M=Ti, V; X=C, N)[J]. Acta Phys. -Chim. Sin., 2017, 33(10): 2022-2028.
[15] Yan-Ting LI,Xin-Min LIU,Rui TIAN,Wu-Quan DING,Wei-Ning XIU,Ling-Ling TANG,Jing ZHANG,Hang LI. An Approach to Estimate the Activation Energy of Cation Exchange Adsorption[J]. Acta Phys. -Chim. Sin., 2017, 33(10): 1998-2003.