| GO 9 | 2025 | Doctor-blade, 3000 ℃ annealing reduction +3000 ℃ second annealing reduction |
| GO 10 | 1940 | Casting, 3000 ℃ annealing reduction |
| GO 48 | 1100 | Evaporation, 2000 ℃ annealing reduction |
| GO 76 | 1283–1434 | Electro-spray deposition,2850 ℃ annealing reduction |
| GO 77 | 1390 | Vacuum filtration, HI reduction |
| Graphene 78 | 1529 | Ball milling,2850 ℃ annealing reduction |
| GO 81 | 1224 | Doctor-blade, film paste Hot pressing + 2800 ℃ annealing reduction |