水系锌二次电池MnO2正极的晶体结构、反应机理及其改性策略
|
|
陈鲜红, 阮鹏超, 吴贤文, 梁叔全, 周江
|
Crystal Structures, Reaction Mechanisms, and Optimization Strategies of MnO2 Cathode for Aqueous Rechargeable Zinc Batteries
|
|
Xianhong Chen, Pengchao Ruan, Xianwen Wu, Shuquan Liang, Jiang Zhou
|
|
图6 (a) PANI-MnO2纳米层结构示意图;(b)经过400 ℃热处理去除PANI后的PANI-MnO2纳米层结构的HR-TEM图像54;(c) cw-MnO2的XRD图案和晶体结构;(d)左图:Zn插层结构和所需的相应能量;右图:锌的球内络合效应导致面向锰的突出,形成放大的Zn-Mn哑铃结构(数字代表原子间的距离) 83;(e)预嵌Na+和水分子的δ-MnO2充放电工作示意图;(f) δ-NMOH电极的非原位XRD图87
|
Fig 6 (a) Schematic diagram of PANI-MnO2 nanolayers structure. (b) HR-TEM image of PANI-MnO2 nanolayers structure after removing PANI by heat treatment at 400 ℃ 54. (c) XRD pattern and crystal structure of cw-MnO2. (d) Left: Zn-intercalation structure and corresponding energy; Right: the inner-sphere complexation of zinc leads to the protrusion of the facing Mn, constituting a Zn-Mn dumbbell structure as zoomed (numbers represents the distance between atoms) 83. (e) Schematic diagram of pre-intercalated Na+ and water molecules δ-MnO2 during charging and discharging. (f) ex situ XRD pattern of δ-NMOH electrode 87.
|
|
|
|
|