物理化学学报 >> 2023, Vol. 39 >> Issue (10): 2305033.doi: 10.3866/PKU.WHXB202305033

所属专题: 北大纳米化学研究中心30周年专刊

通讯 上一篇    下一篇

Pd(100)氧化表面上低温丙烷氧化的活性相研究

徐美佳, 张宇琛, 朱一帆, 李昌林, 吴子昂, 周雄(), 吴凯()   

  • 收稿日期:2023-05-16 录用日期:2023-06-13 发布日期:2023-06-28
  • 通讯作者: 周雄,吴凯 E-mail:xiongzhou@pku.edu.cn;kaiwu@pku.edu.cn
  • 基金资助:
    国家自然科学基金(22222102);国家自然科学基金(21821004);国家自然科学基金(21927901)

Active Phase on Oxidized Pd(100) for Low-Temperature Propane Oxidation

Meijia Xu, Yuchen Zhang, Yifan Zhu, Changlin Li, Zi-Ang Wu, Xiong Zhou(), Kai Wu()   

  • Received:2023-05-16 Accepted:2023-06-13 Published:2023-06-28
  • Contact: Xiong Zhou, Kai Wu E-mail:xiongzhou@pku.edu.cn;kaiwu@pku.edu.cn
  • Supported by:
    the National Natural Science Foundation of China(22222102);the National Natural Science Foundation of China(21821004);the National Natural Science Foundation of China(21927901)

摘要:

钯作为汽车尾气处理的三效催化剂的关键成分,在烷烃的完全氧化和CO低温氧化中扮演着重要催化角色。在富氧环境下,钯表面通常会形成薄的氧化物层。为了揭示钯表面上烷烃完全氧化的活性相,我们对Pd(100)表面氧化过程及其对丙烷氧化的活性相进行了详细研究。实验结果表明,在不同氧化条件下,Pd(100)表面依次形成了三种单层氧化相,即(2 × 2)-O、(5 × 5)-PdO和($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO,它们的O覆盖度分别为0.25单层,0.56单层和0.8单层。值得注意的是,(5 × 5)-PdO结构首次得到了高分辨扫描隧道显微镜成像的确认。实验发现该结构呈现出典型的手性特征,两种手性对映体结构也可在实验中观察到。根据高分辨原子成像,我们提出了新的(5 × 5)-PdO结构模型。(5 × 5)-PdO结构的手性特征在手性催化等领域中可能有着重要意义。热分解实验发现(5 × 5)-PdO结构热分解形成($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO和(2 × 2)-O结构,而($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO热分解产生(2 × 2)-O。该结果表明这些氧化相的热稳定性次序为(2 × 2)-O > ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO > (5 × 5)-PdO。随后我们对比研究了这三种氧化相在低温丙烷氧化方面的催化活性。结果表明,只有($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO可以在接近室温条件下催化丙烷氧化,而($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO出现了大量氧缺陷,且形成还原的(2 × 2)-O相。程序升温脱附谱测到了完全氧化产物H2O和CO2,在285和315 K出现两个主要反应温区。(2 × 2)-O和(5 × 5)-PdO相则无明显的催化活性。($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO相的优异氧化活性可能与($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO结构中较高的O密度相关,即结构中较活泼的O物种。本研究表明($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO为丙烷低温氧化中的活性相。这些有助于人们理解三效催化剂的工作机制,对于高效低温三效催化剂的研发具有重要意义。

关键词: 氧化钯, 手性氧化物, 丙烷低温氧化, 扫描隧道显微镜

Abstract:

Palladium, a key component of three-way catalysts used in automobile exhaust treatment, plays a pivotal role in complete oxidation of alkanes and low-temperature oxidation of CO. Under oxygen-rich conditions, a thin oxide layer spontaneously forms on the palladium surface. To understand the influence of the oxidized palladium surface on the active phase of low-temperature hydrocarbon oxidation, we have conducted a comprehensive study of the oxidation process on Pd(100) and its impact on propane oxidation. Our experimental results reveal that under varying oxidation conditions, the Pd(100) surface sequentially forms three different monolayered oxide phases, namely, (2 × 2)-O, (5 × 5)-PdO and ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO. The oxygen coverage correspondingly increases in the order of 0.25 monolayer, 0.56 monolayer and 0.8 monolayer. Notably, (5 × 5)-PdO is identified for the first time by high-resolution scanning tunneling microscopy. Experiments show this structure exhibits typical chiral features with its two enantiomers observed in the experiments. The chiral features of the (5 × 5)-PdO structure may bear significant implications in practical applications like chiral catalysis. Based on high-resolution atomic imaging, we have proposed a new (5 × 5)-PdO structure model. In addition, it's experimentally revealed that upon thermal treatments the (5 × 5)-PdO structure decomposes into the ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO and the (2 × 2)-O structures, and the ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO decomposes into the (2 × 2)-O structure as well. These results suggest that the thermal stability of these oxide phases is in the order of (2 × 2)-O > ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO > (5 × 5)-PdO. We have also compared the catalytic activities of these three oxidation phases in low-temperature propane oxidation. The results show that only the ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO could catalyze propane oxidation near room temperature. We have observed a significant number of oxygen defects in the ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO, which also forms the reduced (2 × 2)-O phase. Both complete oxidation products H2O and CO2 are detectable by temperature-programmed desorption within two main temperature slots around 285 and 315 K. Neither the (2 × 2)-O nor the (5 × 5)-PdO phase shows an obvious catalytic activity. The superior oxidation activity of the ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO phase might be associated with its higher O density and hence more active O species within the structure. Our study indicates that the ($ \sqrt{\text{5}} $ × $ \sqrt{\text{5}} $) R27°-PdO serves as the active phase for the low-temperature propane oxidation. These insights would help understand the working mechanisms of three-way catalysts and should be of great importance for the development of efficient and low-temperature three-way catalysts.

Key words: Palladium oxide, Chiral oxide, Low-temperature propane oxidation, Scanning tunneling microscopy